| Properties | Unit | F43 |
|---|---|---|
| Density | g/cm³ | 1.8 |
| Flexural Strength | Mpa 20°C ps1 Mpa 4 days @200°C psi |
440 63,800 260 37,700 |
| Flexural Modulus | GPa Psi x 106 Gpa 4 days @200°C Psi x 106 |
22 3.19 20 2.9 |
| Bond Strength | KN @ 7.9 thick | 5.7 |
| Water Swell (24 hr) | % @ 80°C length % @ 80°C thick |
<0.02 <0.02 |
| Vacuum movement (96 hr) |
% @ 125°C length % @ 125°C thick |
<0.02 <0.02 |
| Coefficient of Thermal Expansion | 10-6/°C length 10-6/°C thick |
11 30 |
| Operating Temperature | °C Continuous °C Maximum |
200 225 |
The information contained in this data sheet is presented in good faith. They are typical test results tested generally in accordance with BS 2782 and ASTM test methods and should not be used for specifications. TENMAT does not warrant the conformity of its materials to the listed properties or their suitability for any particular purpose. For further information, please contact TENMAT.